Moisture readings get quoted at owners all the time, usually with no explanation. Here is what the meter is actually measuring, how the readings are taken, what the numbers mean, and when moisture should change your decision about a boat.
A marine moisture meter does not tell you a percentage of water in the laminate in the way a laboratory test would. It measures electrical conductivity or capacitance in the material beneath the probe, and converts that into a comparative reading.
That distinction matters. The reading is relative, not absolute. It is meaningful when compared against a known dry reference point and against other areas of the same hull, not as a standalone number. Two identical meters from different manufacturers can read the same hull quite differently.
This is why a surveyor who simply announces "21 percent" without explaining the reference, the meter used or where the readings were taken is telling you very little.
A defensible moisture assessment is methodical, not a couple of spot checks near the waterline:
On a hauled-out vessel we also tap-test for delamination and inspect the keel, keel bolts, rudder stock and through-hulls, because moisture is only one part of the picture.
The scale most New Zealand surveyors use, and the one we report to, grades readings in three bands:
| Reading | Grade | What it means |
|---|---|---|
| 0 to 10 | Acceptable | Consistent with a dry, sound laminate. Normal for a well maintained GRP hull. |
| 11 to 20 | Monitor | Elevated. Not necessarily a problem, but it warrants investigation: where is it, how widespread, and is there a source such as deck fittings or a repair. |
| 21 percent and above | Action required | High moisture. This is where blistering, delamination and structural concerns become real, and where a buyer needs a repair estimate before committing. |
These bands are a guide, not a verdict. A single high reading under a chainplate or around a stanchion base is usually local ingress from a leaking fitting, which is a straightforward repair. A hull reading consistently high across a wide area below the waterline is a different conversation entirely.
These two get used interchangeably and should not be. Moisture is water present in the laminate. Osmosis is a chemical process: water soluble materials in the laminate draw water in through the gelcoat by osmosis, creating acidic fluid that accumulates and pushes the gelcoat away from the laminate, forming blisters.
A boat can have elevated moisture readings with no osmosis at all. A boat can also have blisters that are cosmetic rather than structural. What determines severity is the extent, the depth, whether the laminate itself is compromised, and whether the blistering is active.
For a buyer, the practical question is not "does it have osmosis" but "what will this cost to fix, and is that reflected in the price".
On many older boats the deck is a bigger issue than the hull. Balsa or ply cores absorb water through failed sealant around fittings, hatches, chainplates and stanchion bases. Once wet, the core can rot, and the deck loses stiffness.
The warning signs are a dull sound when tapped, springiness underfoot, water weeping from fittings, and elevated meter readings around hardware. Repair means removing the skin, replacing the core and re-laminating, which is skilled work and priced accordingly.
This is one of the reasons a survey should include deck readings as standard, not as an optional extra.
For hull moisture and blistering, the usual sequence is: haul out, strip the antifouling and gelcoat in affected areas, allow the laminate to dry to an acceptable level (which can take weeks or months, sometimes under heat or vacuum), then re-laminate and apply an epoxy barrier coat before antifouling.
Costs vary enormously with extent. Localised blister repair on a small area is a modest job. A full hull peel and re-laminate on a 12 metre yacht is a major project. Because the drying time is unpredictable, this is exactly the kind of defect that should be quantified before you buy, not discovered afterwards.
Our moisture and osmosis survey is built around producing that number for you, and it can be commissioned on its own if you already have a survey but want the hull assessed properly.
We test hull, deck and structure, and report what the readings mean in plain language with a repair estimate.
Every survey is carried out by a Class 1 Commercial Marine Engineer: